Tax included.

LiTaO3 crystal often be used to measure the electric field. It pertains to 3m crystal system. Compared to LiNbO3, it possesses higher electro-optic coefficient. Moreover, optical damage threshold, birefringence, transmission band, light transmittance, sensity in measurement ,and the wafer fabrication cost are also the superiority of LiTaO3.

Model
Size(mm)
Orientation
Coating
Price
Delivery
(week)
Order
LN001
9*9*25
z-cut
AR/AR @ 1064 nm, with gold electrodes
510
1-2
LN002
6*6*25
z-cut
AR/AR @ 1065 nm, with gold electrodes
570
1-2
LN003
Ø80*0.6
z-cut
Uncoated
140
1-2
LN004
25.6*25.6*0.5
0/0
Uncoated
90
1-2
LN005
Ø50*0.5
0/0
Uncoated
110
1-2
LN006
Ø100*0.8
z-cut
Uncoated
330
1-2
LN007
3*3*10
z-cut
AR/AR/AU/AU
80
1-2
LN008
9*9*20
z-cut
AR/AR/AU/AU
80
1-2
LN009
Ø50*0.5
0/0
Uncoated
110
1-2
LN010
Ø50*3
0/0
Uncoated
110
1-2
LTB001
Ø2*50
X、Y、Z±1º

Negotiable
1-2
LTB002
Ø3*50
X、Y、Z±1º

Negotiable
1-2
LTW001
10*10*0.5
X, Y, Z or Y rotation with or without locating edges

Negotiable
1-2
LTW002
Ø2*0.5
X, Y, Z or Y rotation with or without locating edges

Negotiable
1-2
LTW003
Ø3*0.5
X, Y, Z or Y rotation with or without locating edges

Negotiable
1-2
LTW004
Ø3*1
X, Y, Z or Y rotation with or without locating edges

Negotiable
1-2

 

Point group C3v-3m
Refractive index at 632.8nm n0=2.176
ne=2.186
Transparent Range 0.4-5.0μm
Orientation X,Z,36°Y,42°Y,128°Y
Melting point 1650℃
Density 7.45g/cm3
Mohs hardness 5.5
Thermal expansion coefficient aa=16×10-6/K, ac=4×10-6/K
Specific heat 0.06J/(kg•°C)
Cell Parameters a=5.154Å,c=13.781Å
Curie Temperature 605℃
Elastic Stiffness Coefficient CE11=2.33(×1011N/m2)
CE33=2.77(×1011N/m2)
Electro-optical coefficients@0.63μm γS13=7×10-12m/V
γS33=30.3×10-12m/V
Heat Capacity (Cp)

100 J / k.mol

 

Go To Crylink Website To Get More Information About This Product.